Reinforcing measures for steel structures
Release Time:
2021-09-15
When the steel structure is damaged, we need to find and solve the problem immediately. The main factors for the damage to the steel structure are: 1) Insufficient bearing capacity of the structure caused by load changes, extended service, and changes in codes and regulations; 2) The components are deformed, twisted, disabled, dented, etc. due to various accidents, resulting in weakened sections of components, warped rods, and cracked connections; 3) Deformation, cracking and warping of components or connections caused by temperature difference; 4) The cross-section of steel structural members is weakened due to corrosion caused by chemical corrosion and electrochemical corrosion; 5) Others include mistakes in design, production, construction, and illegal use and operation during the service period. There are mainly three types of reinforcement technical measures for steel structures: 1) Cross-section reinforcement method: Reinforce with steel in part or along the whole length of the member, and connect them into a whole to make them bear common force; 2) Change the calculation diagram: add additional supports, adjust the load distribution, reduce the level of internal force, force the displacement of the statically indeterminate structural supports, and reduce the stress peak; 3) Prestressed cable method: use high-strength cables to reinforce weak links in the structure or improve the overall bearing capacity, stiffness and stability of the structure.
When the steel structure is damaged, we need to find and solve the problem immediately. The main factors for the damage to the steel structure are:
1) Insufficient bearing capacity of the structure caused by load changes, extended service, and changes in codes and regulations;
2) The components are deformed, twisted, disabled, dented, etc. due to various accidents, resulting in weakened sections of components, warped rods, and cracked connections;
3) Deformation, cracking and warping of components or connections caused by temperature difference;
4) The cross-section of steel structural members is weakened due to corrosion caused by chemical corrosion and electrochemical corrosion;
5) Others include mistakes in design, production, construction, and illegal use and operation during the service period.
There are mainly three types of reinforcement technical measures for steel structures:
1) Cross-section reinforcement method: Reinforce with steel in part or along the whole length of the member, and connect them into a whole to make them bear common force;
2) Change the calculation diagram: add additional supports, adjust the load distribution, reduce the level of internal force, force the displacement of the statically indeterminate structural supports, and reduce the stress peak;
3) Prestressed cable method: use high-strength cables to reinforce weak links in the structure or improve the overall bearing capacity, stiffness and stability of the structure.
Related News

Contact
Address: No. 1, Jinlong Avenue, Jinlong Industrial Park, Xiangyin County, Hunan Province
Tel:0730-2510001
Fax:0730-2510009
Mail:cs-cmc@163.com
Website:www.cmcwelding.com

Messages